Tack Weld: Size, Spacing and Why It Matters
A tack weld is a short, small weld that holds parts in position before the full weld is made. On plate, tacks are typically about 1/2 to 1 in (13 to 25 mm) long and 3 to 6 in (75 to 150 mm) apart; on thin sheet they are small dots about 1 to 2 in (25 to 50 mm) apart. Tack both ends of the joint first, then the middle, so the parts cannot creep out of line.
Every tack becomes part of the finished weld, so it needs the same filler, clean metal and fusion as the weld that covers it.
Tack size and spacing at a glance
| Material | Typical tack length | Typical spacing | Notes |
|---|---|---|---|
| Thin sheet, under 1/8 in (3 mm) | Small dot, about 1/4 in (6 mm) | 1 to 2 in (25 to 50 mm) | Short tacks limit heat and warping |
| Plate, 1/8 to 1/4 in (3 to 6 mm) | 1/2 in (13 mm) | 3 to 4 in (75 to 100 mm) | Tack both ends first |
| Plate, over 1/4 in (6 mm) | 3/4 to 1 in (19 to 25 mm) | 4 to 6 in (100 to 150 mm) | Thick parts pull harder on small tacks |
| Pipe | Short tacks in the root | 3 or 4 around the joint | Spaced evenly to hold the root gap |
These are shop rules of thumb. A welding procedure or drawing that gives tack sizes overrides them.
Why tack welds matter
Tack welds hold the fit-up while you weld. Weld metal shrinks as it cools, and that shrinkage pulls the parts toward the weld. Without enough tacks, a long seam closes up ahead of the arc, the gap disappears, and the joint ends out of square.
Tacks also free your hands. Once the parts are tacked you can take off clamps and welding magnets, check the part with a square, and fix any mistake before the full weld locks it in.
How to tack weld a joint
- Clean the joint to bright metal, including the faces that touch.
- Clamp the parts and set the gap the joint needs.
- Check the fit with a square or a tape.
- Place a tack at one end, then the other end.
- Check the fit again, then add tacks in the middle and work outward, swapping sides on long joints.
- Chip or brush the slag off each tack and look for cracks.
- Grind the start and end of each tack to a taper so the final weld fuses into it.
Use the same settings you will use for the root or first pass. A tack made too cold sits on top of the metal and does not fuse, and the final weld then covers a weak spot.
Tack order and distortion
Tack order controls how the part moves. On a long butt joint, tack the ends, then the center, then halfway between each pair of tacks. On a frame or box, tack every corner lightly before you finish any one corner, and check the diagonals; equal diagonals mean the frame is square.
On thin sheet, short tacks spaced close together limit heat. A long tack on sheet metal can warp the panel before the seam is even started. For more on welding thin and heat-sensitive metal, see how to weld aluminum.
Tack weld vs plug weld vs spot weld
These three welds do different jobs:
| Weld | What it does | Stays in the part? |
|---|---|---|
| Tack weld | Holds parts in place before the full weld | Yes, covered by the final weld |
| Plug weld | Joins overlapping sheets through a hole in the top sheet | Yes, it is the final weld |
| Spot weld | Joins overlapping sheets with a resistance welder | Yes, it is the final weld |
For the overlap joints, see plug weld vs spot weld.
Mistakes to avoid
- Tacking dirty or painted metal, which leaves porosity that the final weld covers.
- Making tacks so small they crack when the part shrinks; make them longer on thick parts.
- Leaving a tall tack in place, which causes a lump or a cold lap in the final bead.
- Forcing badly fitted parts together with tacks instead of refitting them.
A cracked or porous tack shows up later as a flaw in the finished weld. Good vs bad welds shows what to look for.
Safety
Tacking is quick, but the arc is just as bright as a full weld. Wear the helmet down for every tack, and gloves and a jacket. See welding safety tips.
Related guides
Frequently asked questions
Should a tack weld be welded over or ground out?
Either works if the tack is sound. Grind the ends of each tack to a taper so the final weld fuses into it, and grind out any tack that cracked or has porosity.
Why do my tack welds crack?
Tacks cool quickly because they are small, and parts pulling against them as they cool can crack them. Use a slightly longer tack, preheat where the procedure calls for it, and do not force misaligned parts together with the tacks.
Can I tack weld with a different process than the final weld?
Often yes, as long as the tack is sound and compatible with the final weld metal. On code work, the welding procedure says which process and filler the tacks must use.
Related guides
- Guide
How to Weld Aluminum: Welder, MIG and TIG
How to weld aluminum: which welder to use (spool gun MIG or AC TIG), argon gas, filler wire, cleaning off the oxide and settings, step by step for beginners.
- Guide
Can You Weld Galvanized Steel? Fumes and Safe Method
Can you weld galvanized steel? Yes, but the zinc makes harmful fumes. How to grind off the coating, ventilate, protect yourself and weld it safely.
- Guide
Welder Generators: What Size Generator to Run a Welder
What size generator runs a welder: how to read the welder's input amps and volts, running vs surge watts, inverter generators and engine-driven welders.