Good vs Bad Welds: Undercut, Porosity and Other Defects
A good weld has a uniform bead width and ripple, fuses fully into both pieces, blends smoothly at the edges and has no cracks, holes or gaps. A bad weld shows defects such as undercut (a groove at the edge), porosity (pinholes), lack of fusion, overlap, spatter, slag inclusions or cracks, usually from the wrong current, speed, angle, shielding gas or dirty metal.
Good weld vs bad weld at a glance
| Feature | Good weld | Bad weld |
|---|---|---|
| Bead width | Even along the joint | Wavy, narrow or wide in spots |
| Ripples | Evenly spaced | Irregular, lumpy |
| Edges | Blend smoothly into the metal | Groove (undercut) or overlap |
| Surface | Solid, no holes | Pinholes, craters or cracks |
| Fusion | Joins both pieces fully | Edges not melted together |
| Spatter | Little | A lot |
Common weld defects, causes and fixes
| Defect | What it looks like | Common causes | Fix |
|---|---|---|---|
| Undercut | A groove along the toe of the weld | Current too high, travel too fast, arc too long, wrong angle | Lower current, slow down, shorten the arc, pause at the edges |
| Porosity | Pinholes or surface bubbles | Dirty or rusty metal, damp rods, lost gas, wind | Clean to bright metal, dry the rods, check gas and shield from wind |
| Lack of fusion | Weld sits on top without joining | Low current, fast travel, dirty joint | Raise current, slow down, aim the arc at the joint |
| Lack of penetration | The root of the joint is not melted | Low current, tight gap, wrong angle | Increase current or gap, use a proper bevel |
| Overlap (cold lap) | Weld metal rolls over the edge without joining | Travel too slow, current too low | Raise current, speed up |
| Spatter | Droplets around the weld | Arc too long, wrong gas, high wire speed | Shorten the arc, adjust settings |
| Slag inclusion | Slag trapped in the weld | Slag not cleaned between passes | Chip and brush after each pass |
| Cracks | Lines in or beside the weld | Fast cooling, hydrogen, high carbon steel, restraint | Preheat, use dry low-hydrogen rods, grind out and re-weld |
| Burn-through | Holes in thin metal | Current too high, slow travel | Lower current, speed up, use a backing |
Undercut in more detail
Undercut weakens the plate right at the toe of the weld, where stresses concentrate. It is common when the current or the arc length is too great. Reduce current, hold a shorter arc, keep the electrode angle steady and pause slightly at each edge so the weld metal fills the groove. A shallow undercut can be filled with a light extra pass, and deep undercut may need grinding and repair.
Porosity in more detail
Porosity comes from gas bubbles that freeze in the weld. Rust, oil and paint release gas, damp rods release hydrogen and a draft blows away shielding gas. Clean the joint to bright metal, keep rods dry (see 7018 welding rod storage), and weld in a draft-free area when using shielding gas. For wire-feed welders, check that the gas flows and that nothing blocks the nozzle; see what is MIG welding and flux core vs MIG.
Checking your own welds
- Look at the weld with good light after cleaning off slag.
- Check for even width, smooth edges and no holes or cracks.
- Practice on scrap, then break or bend a test piece to see whether the weld has joined the metal.
- Adjust one setting at a time.
Welds on load-bearing parts, pressure vessels and anything where failure causes injury need a qualified inspector and the right code. A home welder’s visual check is not enough for those. For stick setup, see stick welders.
Frequently asked questions
What is undercut in welding?
A groove melted into the base metal along the edge of the weld that the weld metal did not fill. It thins the plate and creates a stress point.
What causes porosity in a weld?
Gas trapped in the weld metal. Common causes are rust, oil or paint on the metal, damp electrodes, lost shielding gas from wind or a leak, and an arc held too long.
How can I tell if a weld is strong?
A uniform bead with full fusion and no visible defects is a good sign, but strength is not proven by looks alone. Structural welds must be inspected or tested to the code that applies.
Can I fix a bad weld?
Many defects can be ground out and re-welded. Cracks must be removed completely first. For structural work, follow the repair procedure the code requires.
Related guides
- Guide
Plug Weld vs Spot Weld: How to Make a Plug Weld
Plug weld vs spot weld: how each joins overlapping sheet, when to use a plug weld with a MIG welder, hole size, step by step, and how to check the result.
- Guide
Welding Rod Sizes and Amperage Chart
Welding rod sizes and amperage chart for 6013 and 7018 stick rods, with the metal thickness each size suits, how to read the rod number, and how to set amps.