How to Weld Aluminum: Welder, MIG and TIG
Aluminum is welded with MIG using a spool gun or push-pull gun, or with TIG on an AC machine, always with pure argon gas. Clean off the oxide layer with a stainless brush used only for aluminum, use 4043 or 5356 filler, and travel faster than on steel because aluminum conducts heat quickly. Flux-core and standard stick rods do not suit aluminum.
Welding aluminum at a glance
| Item | Choice |
|---|---|
| Process | MIG with spool gun, or AC TIG |
| Gas | 100% argon |
| Filler | 4043 or 5356, matched to the alloy |
| Cleaning | Stainless brush used only on aluminum, plus solvent |
| Technique | Push, with fast, steady travel |
| Polarity | MIG on DC electrode positive, TIG on AC |
Why aluminum is harder than steel
- Oxide layer: aluminum oxide melts at a much higher temperature than the metal under it, so it must be cleaned off before welding.
- Heat conduction: the metal moves heat away fast, so it needs higher heat input and quick travel, and can still burn through.
- Soft wire: aluminum wire is soft and buckles in a normal MIG liner.
Step by step
- Choose the process. A MIG welder with a spool gun is the easiest to start with. TIG gives more control but takes more practice. See what is MIG welding and types of welding.
- Use pure argon gas; see shielding gas for MIG.
- Clean the joint with a stainless brush that you use only on aluminum, then wipe off oil with a solvent.
- Set the machine from the maker’s chart for the thickness, and test on scrap.
- Push the gun, not drag it, with a steady travel speed.
- Watch the pool, and stop at the end of the bead so you don’t leave a crater.
Common problems
- Black, sooty weld: dirty metal, wrong gas or too slow a travel.
- Porosity: moisture, oil or poor gas coverage.
- Burn-through: too much heat or too slow a travel. See good vs bad welds.
Safety
Wear a helmet with the right shade, gloves and a jacket. See welding helmets and welding safety tips. Aluminum welds bright, so a proper shade matters.
Frequently asked questions
Can I weld aluminum with a regular MIG welder?
Not easily. Soft aluminum wire tangles in a standard gun, so use a spool gun or a push-pull gun. Many small MIG welders accept a spool gun.
What gas for aluminum MIG welding?
Pure argon. CO2 mixes cause porosity and a dirty weld.
What filler wire do I use on aluminum?
4043 is a common general-purpose filler, and 5356 suits stronger welds and some marine and anodizing jobs. Match the filler to the alloy using the wire maker's chart.
Why does aluminum burn through so easily?
It conducts heat quickly and has no color change before it melts. Control the heat with travel speed and settings, and practice on scrap.
Related guides
- Guide
Can You Weld Galvanized Steel? Fumes and Safe Method
Can you weld galvanized steel? Yes, but the zinc makes harmful fumes. How to grind off the coating, ventilate, protect yourself and weld it safely.
- Guide
Welder Generators: What Size Generator to Run a Welder
What size generator runs a welder: how to read the welder's input amps and volts, running vs surge watts, inverter generators and engine-driven welders.
- Guide
Welding Magnets: Types, Angles and Holding Force
Welding magnets compared: arrow, switchable and adjustable-angle types, 45, 90 and 135 degree holds, holding force ratings, heat limits and how to use them.